42CrMo hot rolled steel sheet/bar
42CrMo steelbelongs to plastic mold steel in mold steel from the perspective of material classification. It has good mechanical properties and machinability, and is widely used. There are mainly two types of materials, plate and round bar. Plate is used for mold processing Production, round rods are used to machine parts directly, which has been recognized by the industry.
Key words:
42CrMo hot rolled steel sheet/bar
Classification:
Description
Product introduction
42CrMo4 is a steel for quenching and tempering, which has a good combination of strength and toughness in the quenched and tempered condition. After the oil quenching, the steel will be through hardened up to ø60 mm bar diameter. The microstructure of larger dimensions is not fully martensite. The steel is applicable to induction hardening. The surface hardness will exceed min. 53 HRC. 42CrMo4 can be delivered M-treated in order to optimize the machinability.
Technical data
| Chemical Composition | ||||||||
| Steel Grade | C | Si | Mn | P | S | Cr | Mo | Cu |
| 35CrMo | 0.38~0.45% | 0.17~0.37% | 0.50~0.80% | ≤0.035% | ≤0.035% | 0.90~1.20% | 0.15~0.25% | ≤0.30% |
Mechanical properties
| Yield strength σs/MPa (>=) | Tensile strength σb/MPa (>=) | Elongation δ5/% (>=) |
Reduction of area ψ/% (>=) |
Impact absorbing energy Aku2/J (>=) | Hardness HBS 100/3000 max |
| ≥930(95) | ≥1080(110) | ≥12 | ≥45 | ≥78(8) | ≤217HB |
In order to increase the die life to more than 800,000 die times, the pre-hardened steel can be hardened by quenching and low temperature tempering. When quenching, preheat at 500-600℃ for 2-4 hours, and then keep it at 850-880℃ for a certain period of time (at least 2 hours), then put it in oil and cool to 50-100℃ and air cooling, the hardness can reach 50 after quenching -52HRC, in order to prevent cracking, 200℃ low temperature tempering treatment should be carried out immediately. After tempering, the hardness can be maintained above 48HRC.
42CrMo Steel Heat Treatment
Annealing
Annealing in 760±10℃, furnace cooling to 400℃ then air cooling.
Normalizing
Normalizing in 760±10℃, air cooling after out of the furnace.
Notes About Quenching and Tempering Treatment
Must pay attention to the temperature of liquid coolant. And must make sure there are no oil contamination or other impurities. Otherwise, the hardness of steel will be not enough or out of the balance.
Quenching and tempering for billet steel material without processing, then it will get non-uniform hardness. So processing of forging or grinding is necessary before the Q+T.
Qualification
Strength
Related Products
Consultation
Please leave your contact information and we will get back to you as soon as possible
zan_yang@steelaotong.com
Address:29th Floor, West Block A, Century Apartment, Gangcheng Street, Haigang District, Qinhuangdao City
Copyright © 2025 Qinhuangdao Aotong Trading Co., Ltd.