18CrNiMo7-6 hot rolled steel round bars
18CrNiMo7-6 is a case hardening steel with high toughness. There are a number of variants with high cleanliness requirements. All variants possess tighter composition ranges compared to the standard. produced with the quality class IQ (isotropic quality). This ensures a very low number of elongated sulphide inclusions which will give more isotropic properties. The high oxidic cleanliness will enable the steel to meet the same high cleanliness demands as for re-melted qualities
Key words:
18CrNiMo7-6 hot rolled steel round bars
Classification:
Description
Product introduction
18CrNiMo7-6 hot rolled steel round bars information
18CrNiMo7-6 is a case hardening steel with high toughness. There are a number of variants with high cleanliness requirements. All variants possess tighter composition ranges compared to the standard. produced with the quality class IQ (isotropic quality). This ensures a very low number of elongated sulphide inclusions which will give more isotropic properties. The high oxidic cleanliness will enable the steel to meet the same high cleanliness demands as for re-melted qualities
Product parameters
Chemical Composition
| Standard | Grade | C | Mn | P | S | Si | Ni | Cr | Mo |
EN 10084 |
18CrNiMo7-6 | 0.15-0.21 |
0.50-0.90 |
≤ 0.025 |
≤ 0.035 |
≤ 0.04 |
1.4-1.7 |
1.5-1.8 |
0.25-0.35 |
| 1.6587 |
Physical Property
| Density, g/cm3 | 7.85 | ||||
| Specific heat capacity J/(kg.K) | 460 | ||||
| Electric resistivity Ohm.mm2 /m | 0.18 | ||||
| Electric conductivity Siemens.m/mm2 | 5.55 | ||||
| Modulus of elasticity Gpa | 210 | ||||
| Thermal expansion 10^6 m/(m.K) | 100 ℃ | 200 ℃ | 300 ℃ | 400 ℃ | 500 ℃ |
| 11.1 | 12.1 | 12.9 | 13.5 | 13.9 | |
Mechanical Property
| Size mm | ≤ 11 | 12-30 | 31-63 |
| R Mpa | 1180-1420 | 1080-1320 | 980-1270 |
| Rp 0.2 Mpa | ≥ 835 | ≥785 | ≥ 685 |
| A % | ≥ 7 | ≥ 8 | ≥ 5 |
| C % | ≥ 30 | ≥ 35 | ≥ 35 |
| Kv J | ≥ 44 | ≥ 44 | |
| Hardness HB | 354-406 | 327-384 | 295-373 |
Forging
DIN 1.6587 | 17CrNiMo6 |18CrNiMo7-6 forging temperature:900 – 1100°C,cool slowly in the sand after forged.
Heat Treatment
- Normalizing:850 – 880°C/air
- Soft annealing:650 – 700°C/furnace
- Stress relieve:630- 650oC
- Carburising:880 – 980°C
- Core hardening:830 – 870°C/water
- Intermediate annealing:630 – 650°C
- Case hardening:780 – 820°C/water
- Tempering:150 – 200°C
Surface Hardness
- Treated to improveshearability(+S):Max 255HB
- Soft annealed(+A):Max 229HB
- Treated to hardness range(+TH):179-229HB
- Treated to ferrite-pearlite structure and hardness range(+FP):159-207HB
Application
DIN 1.6587 | 17CrNiMo6 |18CrNiMo7-6 steel for the parts which require core tensile strength and high hardness. Susceptible to the large seized parts with high wearing resistance and loading such as: Heavy Duty Bushings and Bearings, Cam Followers, Clutch Dogs, Compressor Bolts, Extractors, Fan Shafts, Heavy Duty Gears, Pump Shafts, Sprockets, Tappets, Wear Pins, Wire Guides etc..
Qualification
Strength
Related Products
Consultation
Please leave your contact information and we will get back to you as soon as possible
zan_yang@steelaotong.com
Address:29th Floor, West Block A, Century Apartment, Gangcheng Street, Haigang District, Qinhuangdao City
Copyright © 2025 Qinhuangdao Aotong Trading Co., Ltd.